Various abnormalities and causes of pet bottles

A, coking: 1 bottle embryo temperature is too high 2 blower blower power is too small, wind uneven
B. Inhomogeneous thickness: The uneven output power of the corresponding heating lamp causes partial uneven heating. With pre-blowing time, pre-blowing position, pre-blowing pressure are related.
C, bottle support ring bruises: preform embryo output guide, into the embryo transfer turntable, pull guide block robot, the corresponding position of the bottle guide block normal operation
D, bottle capacity is too small (large): pre-blowing time and blowing time is too long, the mold temperature is set too low temperature bottle capacity is small, the opposite is large.


E, the bottle has oil: no replacement after the mold replacement

F, bottle height ranging: 1 different mold manufacturing 2 mold temperature is too low, uneven bottle thickness caused by bottle shrinkage when the bottle is sterilized too

G. Small dents in the bottle are not smooth: There are substances inside the mold.

H, bottle white: bottle heating temperature is too low, local: the corresponding heating lamp output power is too small, all: the preform temperature is set too low

I. Bottle neck concave eccentricity: 1 Out of the bottle conveying carousel is in the wrong position 2 The guide block of the bottle is uneven and the clearance is too small 3 The conveying wind is too small, the bottle conveying is not smooth and it is conveyed by the transfer carousel.
J. There is a small amount of material in the neck of the bottle: there is condensate inside the mold.

More PET bottle content please pay attention --- PET bottle channel

The Food Industry Network prohibits the reprinting of articles on this site. Other sites must contact the site before reprinting and despise shameless theft.

Briefcase

Briefcase,Leather Briefcase,Briefcase For Men,Brief Case

Ningbo Fineweather International Trade Co., Ltd. , https://www.finewbag.com